Energy & PowerSteam Turbine

Steam turbine casing (inner / outer, HP & LP cylinders)

ASME B31.1 / EN 13480. Cr-Mo grades: PWHT mandatory. High-temp tensile & creep rupture data per EN 10302. IBR (Indian) / TÜV / CE marking as applicable. Operating temperature up to 565°C HP.

Request Quote
Steam turbine casing (inner / outer, HP & LP cylinders)

Specifications

Material
Cr-Mo cast steel: ASTM A217 WC9 (Cr2.25Mo1) / WC6 (Cr1.25Mo0.5); ASTM A356 Gr10 for large LP casings
Grades
WC9;WC6
Material Class
Cr-MoCast Steel
Applicable Standards
ASTM A217ASTM A356 Gr10ASME B31.1EN 13480EN 10302IBR
Service Conditions
high temperature
Common Processes
Resin sand / furan no-bake (large complex geometry); shell moulding (selected sections); heat treat (N&T)
NDT & Inspection
RT (100% critical sections, ASTM E94); UT (wall thickness, internal defects); MT; hydrostatic steam test; dimensional CMM; hardness (HB 150–250)
Typical Specs & Notes
ASME B31.1 / EN 13480. Cr-Mo grades: PWHT mandatory. High-temp tensile & creep rupture data per EN 10302. IBR (Indian) / TÜV / CE marking as applicable. Operating temperature up to 565°C HP.
Caveats
Cr-Mo grades: PWHT mandatory.

Need this product?

Submit your quantity and drawing — we'll quote within 48 hours.

Request Quote
Cast To Your Spec

Don't See Your Part? We'll Cast It From Your Drawing.

Send a drawing, sample, or spec and we'll cast it in the right alloy from 25 to 5,000 kg, then machine and inspect it to print. Quote back in 48 hours, no minimum order.

48-hour quote turnaroundNo minimum order quantityIron, carbon, stainless & duplexISO 9001 certified
CallRFQGet a QuoteEmail