CementClinker Cooler

Clinker breaker hammer (clinker size reduction before cooler)

Clinker temperature: 200–600°C at breaker entry. Material must handle impact at elevated temperature. Mn steel: hardness reduces at >300°C – Hi-Cr white iron preferred for high-temp breakers.

Request Quote
Clinker breaker hammer (clinker size reduction before cooler) hero

Specifications

Material
Hadfield Mn steel Mn14Cr2 / Mn18Cr2 (impact dominant); Hi-Cr white iron 27%Cr (abrasion dominant)
Grades
Mn14Cr2;Mn18Cr2
Material Class
HadfieldWhite IronMn Steel
Service Conditions
high temperatureabrasionimpact loading
Common Processes
Sand casting; heat treat (Mn: solution anneal; Hi-Cr: destabilise + temper)
NDT & Inspection
Chemical analysis; hardness; microstructure; dimensional; Charpy (Mn); VT
Typical Specs & Notes
Clinker temperature: 200–600°C at breaker entry. Material must handle impact at elevated temperature. Mn steel: hardness reduces at >300°C – Hi-Cr white iron preferred for high-temp breakers.
Caveats
Material must handle impact at elevated temperature.

Need this product?

Submit your quantity and drawing — we'll quote within 48 hours.

Request Quote
Cast To Your Spec

Don't See Your Part? We'll Cast It From Your Drawing.

Send a drawing, sample, or spec and we'll cast it in the right alloy from 25 to 5,000 kg, then machine and inspect it to print. Quote back in 48 hours, no minimum order.

48-hour quote turnaroundNo minimum order quantityIron, carbon, stainless & duplexISO 9001 certified
CallRFQGet a QuoteEmail